Glass Types for Office Partitions: Toughened, Laminated, Acoustic and Low Iron Explained

About Us » Knowledge Hub » Office Partitioning » Glass Types for Office Partitions: Toughened, Laminated, Acoustic and Low Iron Explained
Jin Li, Group Principal Structural Engineer at Radii Planet Group

By Jin Li
Group Principal Structural Engineer, Radii Planet Group
Reviewed by James Marchant, Group Senior Product Manager
Published 18 November 2026 | Review due 17 November 2027

Toughened, laminated, acoustic laminated and low iron glass look almost identical when they arrive on site. Once installed, they behave very differently. Here's how each glass type is made, how it breaks, what it does for acoustics and where it fits in an office fit-out.

The partition system you choose sets the framework: single or double glazed, framed or frameless, the profile width and the doors it takes. The glass inside that framework decides how safe the screen is, how much sound it stops and how true its colour looks.

The clearest way to see the difference between glass types is to look at how each one breaks.

If you're still choosing a system, start with our office glass partitions guide or our comparison of framed and frameless glass partitions.

Four glass panes break in turn: annealed into large sharp shards, heat strengthened into larger pieces, toughened into small blunt fragments, and laminated cracking but staying in place on its interlayer.


Where it starts: annealed float glass

Almost all flat glass begins as float glass. Silica sand, soda ash and limestone are melted at around 1,550°C together with recycled glass, known in the industry as cullet. The molten glass flows onto a bath of molten tin, which gives it a flat, optically smooth surface. Its thickness is set by the speed at which the glass is drawn along the bath: the faster it's pulled, the thinner the glass. It's then cooled slowly in an annealing lehr. The result is annealed glass, typically produced in thicknesses between 3mm and 25mm.

Annealed glass is the raw material for every other type in this article, but on its own it isn't a safety glass. When it breaks, it forms large, sharp, jagged shards, often in a starburst pattern from the point of impact. That makes it generally unsuitable for the critical locations defined in building regulations, which take in any full-height partition glazing that runs below 800mm from the floor.


Toughened glass and heat soaking

Toughened glass is annealed glass that has been heated to around 650°C and then cooled rapidly with jets of air. The surfaces cool and set first, which locks them into compression while the core stays in tension. That balance of stresses makes toughened glass considerably stronger than annealed glass of the same thickness.

When toughened glass does break, the stored energy releases all at once and the pane shatters into thousands of small, blunt-edged pieces. That break pattern is what makes it a safety glass.

The same stress balance also sets a limit. Once glass is toughened, it can't be cut, drilled or edge-worked, because breaching the tensioned core causes the whole pane to fail. Holes for patch fittings, notches and cut-outs for door hardware all have to be made before toughening, so dimensions need to be fixed early.

Where toughened glass works best

  • Frameless glass doors, where strength at the fixings matters
  • Panels that need holes or notches for hardware
  • Guarding, where it's used as toughened laminated glass

Heat strengthened glass

Made to BS EN 1863-1 using the same process with slower cooling. It's stronger than annealed glass but still breaks into relatively large, sharp fragments, so it isn't generally classed as a safety glass on its own and is normally used as part of a laminated build-up.

Heat soaking and spontaneous breakage

Very occasionally, a toughened pane breaks with no obvious impact. The usual cause is a nickel sulphide inclusion, a tiny impurity that can form during glass manufacture. Rapid cooling during toughening can trap it in an unstable state, and over time it may expand enough to crack the pane.

Heat soak testing to BS EN 14179-1:2016 reheats toughened glass and holds it at around 260°C for at least two hours, so that panes containing these inclusions fail in the factory rather than in a finished meeting room. With heating and cooling, a full cycle takes several hours, so allow for it in lead times. It significantly reduces the risk, though it doesn't remove it completely, and it can't protect against edge damage during handling or installation.

For toughened glass in partitions and doors, heat soaking is highly recommended.

Toughened panes pass through a heat soak oven. One pane containing a nickel sulphide inclusion breaks inside the oven, and the remaining panes continue to site.

Laminated glass

Laminated glass bonds two or more panes together with a plastic interlayer. The panes can be annealed or toughened, which changes how the glass behaves. If the glass breaks, the fragments stay bonded to the interlayer and the pane tends to stay in place rather than falling out. Laminated glass generally provides improved post-breakage containment, as fragments tend to remain bonded to the interlayer. Laminated glass may be classified as safety glass where it achieves the appropriate impact classification under BS EN 12600. The classification depends on the glass construction, interlayer properties and tested performance.

It's described by its layers. Two panes with one interlayer is known as three-ply. A common partition build-up is two 6mm panes with a 0.8mm acoustic interlayer, giving a total thickness of 12.8mm.

Exploded section of a 6mm pane, a 0.8mm acoustic interlayer and a second 6mm pane coming together as 12.8mm acoustic laminated glass, which then cracks but stays held on the interlayer.

Interlayer options

  • PVB (polyvinyl butyral): the most common interlayer for general partition glazing.
  • Acoustic PVB: a modified PVB that damps sound vibration (see the next section).
  • EVA (ethylene-vinyl acetate): used for decorative builds that encapsulate fabrics or meshes, and where edges may be exposed to moisture.
  • SGP (SentryGlas® Plus): a stiffer ionoplast interlayer, used where the glass needs to keep structural capacity after breakage.
  • Coloured interlayers: such as Vanceva, tint the glass from within, so the colour can't scratch or peel. Available in non fire rated glazing.
  • Annealed laminated: the standard choice for framed partitions. Our partitions use it in 10.8mm, 12.8mm, 14.8mm and 16.8mm build-ups. It can be cut and worked after laminating.
  • Toughened laminated: toughened panes laminated together, combining the strength of toughened glass with the post-breakage containment of laminated glass. It's the usual route for guarding and exposed edges. As with any toughened glass, all cutting and drilling has to be done before toughening.

Where a laminated edge is left exposed, the interlayer shows as a fine line along it. In a framed partition the edge is hidden in the profile, which is one reason laminated glass performs at its best in a frame. Depending on the build-up and performance level specified, it can also provide security and UV protection.


Acoustic laminated glass and Rw ratings

Acoustic laminated glass uses a specially formulated interlayer that damps vibration as sound passes through the pane. At the same thickness, it performs better acoustically than standard laminated glass. That makes it the most common route to higher acoustic performance in single glazed partitions, and double glazed systems often use it on both sides of the cavity.

What an Rw rating tells you

Rw is the weighted sound reduction index: a single-number rating of how much sound a construction blocks. It's measured in a laboratory to BS EN ISO 10140-2:2021 and rated to BS EN ISO 717-1:2020. A higher number means better sound insulation.

Because the decibel scale is logarithmic, small differences matter more than they look. An increase of 10 dB represents a tenfold increase in sound intensity, and is generally heard as roughly half as loud.

The glass is only part of the answer

Rw is a laboratory figure. On site, sound finds its way around the glass through ceiling voids, floor voids, façade mullions and door seals, so the on-site result (DnT,w) is normally lower than the laboratory rating.

Head details, ceiling and floor void barriers, door frame seals, drop-down door seals and the door leaf itself all need to be considered alongside the glass.

In double glazed systems, a wider cavity between the panes improves performance, so a wide double glazed partition will generally outperform a slim one.

Section through two rooms showing a partition rated 50 dB Rw in the lab, then sound paths through the ceiling void, floor void, façade mullion and door lowering the on-site result. Illustrative figures.

Across our double glazed range

Zoned by room use

For a leading City of London law firm, single glazed partitions achieved Rw 41 dB, double glazed Rw 45 dB, and an uprated double glazed system Rw 48 dB. Glazed sliding doors rated at Rw 38 dB were used across more than 90 offices and meeting rooms.


Low iron and low carbon glass

The iron naturally present in glass gives standard clear glass a slight green tint. It's most visible at the edges and in thicker build-ups, so acoustic laminated and double glazed partitions show it more than a single thin pane. Modern standard float contains less iron than it used to, and some manufacturers now call it mid-iron glass, but the tint can still show.

Low iron glass has its iron content reduced further, giving a more neutral appearance with truer colour. It matters most for back-painted glass, coloured manifestation that needs to match a palette, and feature glazing where what's behind the glass needs to read accurately. It costs more than standard clear glass, so it's usually specified where colour is part of the design intent.

Two glass panes side by side. Standard clear glass shows a green tint at the edge and over a white back-painted panel, while low iron glass appears neutral.

Low carbon glass

Low carbon glass is made using the same float process as standard glass and has the same appearance and performance. The difference is in how it's produced. A higher proportion of cullet means less energy is needed for melting, because recycled glass has already been through the melting reactions. Some manufacturers are also moving from gas-fired furnaces to electric melting or hydrogen.

Reductions in embodied carbon vary by manufacturer and product, so ask for a product-specific Environmental Product Declaration (EPD) rather than relying on a general claim. Where it's verified, low carbon glass may support credits under BREEAM UK New Construction v6 (Mat 01 and Mat 02) and LEED v5 (MRc2 and MRc4), depending on the project's assessment scope.


Decorative and curved glass

Decorative glass builds privacy and texture into the glass itself, so the effect won't scratch off or lift at the edges the way an applied film can.

  • Reeded and fluted: vertical or horizontal ribs that distort but still read as transparent.
  • Acid-etched and sandblasted: diffuse the view.
  • Back-painted: fully opaque, in any RAL or bespoke colour.
  • Coloured or patterned interlayers: built into laminated glass.
  • Digitally printed graphics: on optically clear film.

Pin down the level of obscuration early, because these finishes give very different privacy outcomes. Rib direction changes the effect, so state it on the drawings. Textured and cast glass also has wider thickness tolerances than float glass, which the framing needs to accommodate. Decorative glass still needs to be safety glass in critical locations, and a decorative finish doesn't automatically meet the manifestation requirements.

Curved glass

Annealed glass gives the most flexibility for tight radii and complex curves, and laminated glass can also achieve relatively tight radii when made from suitably curved plies. Toughened glass is usually limited to single curvature with larger minimum radii, although specialist processes can allow more complex shapes. Fire-rated and acoustic options are also limited in curved form. Where a design needs one of those, a faceted run of flat panes is often the practical route. Decide early whether a true curve is needed, because that choice narrows the glass options for the rest of the project.


Glass types at a glance

Glass type How it breaks Safety glass Best for Watch for
Annealed (float) Large, sharp shards No The base material for processing Not used on its own in partition critical locations
Toughened Small, blunt-edged pieces Yes, typically 1(C)1 Frameless doors, panels with holes or notches Can't be cut or drilled after toughening
Heat soaked toughened As toughened Yes, typically 1(C)1 Toughened glass in partitions and doors Greatly reduces the risk of spontaneous breakage, but doesn't remove it
Laminated Cracks but stays held on the interlayer Yes, typically 1(B)1 Framed partitions, security, post-breakage containment Interlayer visible on exposed edges
Toughened laminated Small pieces held on the interlayer Yes Guarding and exposed edges needing strength and containment All processing done before toughening
Acoustic laminated As laminated Yes Meeting rooms, offices, anywhere speech privacy matters On-site results depend on the whole assembly
Low iron Depends on processing When toughened or laminated Back-painted glass, coloured graphics, feature glazing Higher cost than standard clear

Safety glass in partitions: the essentials

In England, Approved Document K (Section 5) covers protection against impact with glazing, with detailed guidance in BS 6262-4:2018. In Wales, the equivalent guidance is Approved Document N. Glass in critical locations must break safely, resist impact, or fall within set size and thickness limits. In an office, critical locations include:

  • Glazing in doors and side panels below 1500mm above finished floor level.
  • Glazing in walls and partitions below 800mm above finished floor level.

Safety glass is classified by a pendulum impact test to BS EN 12600:2002. Toughened glass typically achieves 1(C)1 and laminated glass 1(B)1. Annealed glass breaks as Type A, so it's generally unsuitable in critical locations.

The classification 1(B)1 decoded: 1 is the highest drop height passed, 1200mm; B means the glass broke but held together on an interlayer; the final 1 is the highest drop height at which it did not break or broke safely.


Choosing the right glass

Glass choices affect acoustics, appearance, cost and lead times, so they're easiest to get right early in the design. Our glass partitions are available in single and double glazed systems with a range of glass build-ups and finishes.

If you're specifying glass partitions, our team can talk through your project.

Talk to our team


This article is general guidance. It's not project-specific advice. Always check the current Building Regulations guidance and confirm glass specifications with the project design team.

Glass Types for Office Partitions: Frequently Asked Questions

Quick answers on toughened, laminated and acoustic glass for office partitions, from thickness to heat soaking.

What type of glass is used for office partitions?

Office partitions use safety glass, which in practice means toughened or laminated glass. Framed partitions commonly use laminated or acoustic laminated glass, while frameless doors and panels that need holes for fittings typically use toughened glass. Annealed glass isn’t used on its own in partition critical locations.

Is toughened or laminated glass better for glass partitions?

It depends on the application. Toughened glass is stronger and suits frameless doors and drilled panels, but it shatters completely if broken. Laminated glass stays in place after breaking, can be acoustic, and suits framed partitions. Toughened laminated glass combines the two where both strength and containment are needed.

How thick is glass in an office partition?

Our partitions use annealed laminated glass in 10.8mm, 12.8mm, 14.8mm and 16.8mm thicknesses, with 12.8mm acoustic laminated a common single glazed build-up. Glass that has to resist barrier loading, crowd loading or wind, such as atrium screens, void protection and balustrades, moves into structural glazing, which needs project-specific structural calculations and engineer sign-off.

Can toughened glass be cut or drilled?

No. Toughened glass can’t be cut, drilled or edge-worked after toughening, because breaching the tensioned core causes the whole pane to shatter. All holes, notches and cut-outs must be made before the glass is toughened.

What is heat soaked glass?

Heat soaked glass is toughened glass that has been reheated and held at around 260°C for at least two hours, to BS EN 14179-1:2016. The process encourages panes containing nickel sulphide inclusions to fail before installation, which significantly reduces the risk of spontaneous breakage on site.

Does thicker glass always mean better acoustics?

Not on its own. An acoustic interlayer, the width of the cavity in double glazing, and the seals and detailing around the glass all have a significant effect. A well-detailed partition with acoustic laminated glass will usually outperform a thicker pane in a poorly sealed frame.